Posted by: Dogbert0051 at Mon Apr 18 00:24:51 2005 [ Email Message ] [ Show All Posts by Dogbert0051 ] 100% silicone is definately the product to use, but you need to wait WAYYYY longer than one day! We're talking about probably 3-4 weeks to let the product completely outgas. What I would reccomend is GE Silicone 2. not silcone 1. The silicone 1 is a latex/silicone blend, silicone 2 is 100% silicone. The only one you can use safely with only letting outgas for a number of days is the one designed for fishtanks. Even then, you need to wait at least a week. | ||